Shanghai Creation GroupCo., Ltd. is a benchmark enterprise of domestic cold heading wire rod, with an average of more than 15 years of industry experience in production management. Most of its cooperative customers are first-class suppliers of global automobile enterprises, and all raw materials come from well-known domestic steel mills. All production orders are 100 per cent traceable.
Technical delivery conditions
: Cold drawing spheroidizing annealing light drawing (spheroidizing annealing light drawing)- SALD
: Annealing cold drawing spheroidizing annealing light drawing state (annealing spheroidizing annealing light drawing)- ASALD;
Surface quality
- : Continuous smooth wire surface
- : No seams, overlaps, pits, scratches and pull marks
- : No rust
Application Industry
- : Automotive industry
- : building materials industry
- : Machinery and equipment industry
- : Other Industries