test页面
COLD FORMING MATERIALS
SAE 1019 cold heading steel wire
MATERIALSENGINEERINGCREATION GROUP
CREATION GROUP / EN

SAE 1019 cold heading steel wire
Steel Grades Chemical Composition
| ID | Grade | C | Si | Mn | P | S | Cr | Mo | B | Alt | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 15 | SAE1019 | 0.15~0.20 | ≤0.10 | 0.60~0.90 | ≤0.020 | ≤0.020 | - | - | - | ≥0.020 | - |
| 23 | SAE1020 | 0.18~0.23 | 0.10~0.35 | 0.30~0.60 | ≤0.020 | ≤0.020 | - | - | - | - | - |
| 45 | SAE1045 | 0.42~0.48 | 0.15~0.35 | 0.60~0.90 | ≤0.020 | ≤0.020 | - | - | - | - | - |
| 49 | 10B16 | 0.13~0.18 | ≤0.10 | 0.80~1.10 | ≤0.020 | ≤0.020 | ≤0.15 | ≤0.04 | 0.0005~0.0030 | ≥0.020 | Ti: 0.01~0.05; Ni≤0.15; Cu≤0.20; Sn≤0.02; N≤0.0080 |
Appearance inspection-acid
Appearance Inspection-Site
Cold upset test
Metallographic examination (100×)
Metallographic examination (500×)
Metallographic inspection equipment
Mechanical property testing-tensile test
Hardness test-HV Vickers
Hardness test-HRB
Hardness test-HRC Rockwell
Chemical Composition-Spectrometer Photo
Membrane test-electron micrograph
Dimensions-Micrometer
Section shape inspection
Corrosion resistance test
Surface roughness test
1、 Roll
Wire bundling example
2、 long strip
Wire bundling example
3、 Export wooden box packaging
Wire bundling example
4、 Photo of loading cabinet
Photo of loading cabinet
5、 Product protection details
Product protection
5、 Product protection details
Product protection
Example of outer packaging
End-face wood packaging
winding packing
PP bag bagging packaging
Wire rack packaging