diameter: 0.40-46mm
tensile strength: refer to technical information

Shanghai Chuang Group is a benchmark company in China focusing on cold-rolled high-quality steel wire. The entire management team has 20 years of industry experience. We have established good relationships with many first-level suppliers in the automotive industry, and all steel wires come from brand steel mills. All orders are 100% traceable.

img1 img1 img1

Specification

+AR

+AC or +AC+PE

+AR+C

+AR+C+AC

+AR+C+AC+LC

+AC+C

img1 img1 img1

Specification

-:continuous and smooth

-:No seams, overlaps, pits, scratches and drawing scars

-:free from rust

img1 img1 img1
img1 img1 img1

Specification

-:automobile industry

-:construction industry

-:machinery industry

-:other industries

img1 img1 img1
Case Study

Products & Service

Related Products

22 MnR4 CHQ wire

Prepainted Aluminium Coil

22 MnR4 CHQ wire

Prepainted Aluminium Coil

22 MnR4 CHQ wire

Prepainted Aluminium Coil

1. Delivery terms combination

Table B.1 -Combination of heat treatment conditions, product form and applicable requirements at the time of delivery

Heat-treatment condition at deliverySymbolProducts form aApplicable requirements in cases where the steel concerned has been ordered with reference to the steel names indicated in
Wire rodBarWireTablesB.2,B.3,B.4 or B.5TablesB.2,B.3,B.4,B.5,B.6 or B,7Optional
As hot-rolled or peeled+AR or +PEXXXChemical composition as specified in Table B.2Mechanical  properties as specified in TablesB.3,B.4 and B.5Chemical compositior as specified in Table B.2Mechanical  properties as specified inTablesB,3,B.4 and B.5Values for hardenability according to Tables B.6 and B.7Supplementa- ry or special requirements as specified in Annex Eh
Cold drawn+AR+C-XX
Cold drawn + spheroidized+AR+C+AC-XX
Cold drawn + spheroidized+skin passed+AR+C+AC +LC-XX
Spheroidized or spheroidized+peeled+AC or +AC +PEXXX
Spheroidized+cold drawn+AC+C XX
Treated to ferrite- pearlite structure and hardness range+FP-X-
OthersOther delivery conditions may be agreed at the time of ordering
a X=applicable,-=not applicable. b If agreed at the time of the enquiry and order.

2. chemical composition

Table B.2 -Chemical composition of steel for surface hardening (suitable for casting analysis)

Steel name b% mass fraction a
  C  Si c  Mn  P    S  Cr  Ni  Mo  B  Cu
Non-alloy steel grades
C10E2C0,08 to 0,120,300,30 to 0,600,0250,025  0,25
C15E2C0,13 to 0,170,300,30 to 0,600,0250,025 0,25
C17E2C0,15 to 0,190,300,60 to 0,900,0250,025 0,25
C20E2C0,18 to 0,220,300,30 to 0,600,0250,025 0,25
Alloy steel grades
18MnB40,16 to 0,200,300,90 to 1,200,0250,025 0,0008 to 0,0050,25
22MnR40,20 to 0,240,300,90 to 1,200,0250,025——0,0008 to 0,0050,25
17Cr30,12 to 0,200,300,60 to 0,900,0250,0250,70 to 1,250,25
17CrS30,12 to 0,200,300,60 to 0,900,0250,020 to 0,0400,70 to 1,250,25
20Cr40,17 to 0,230,300,60 to 0,900,0250,0250,90 to 1,200,25
20CrS40,17 to 0,230,300,60 to 0,900,0250,020 to 0,0400,90 to 1,200,25
16MnCr50,14 to 0,190,301,00 to 1,300,0250,0250,80 to 1,10 0,25
16MnCrS50,14 to 0,190,301,00 to 1,300,0250,020 to 0,0400,80 to 1,10 0,25
16MnCrB50,14 to 0,190,301,00 to 1,300,0250,0250,80 to 1,100,0008 to 0,0050,25
20MnCrS50,17 to 0,220,301,10 to 1,400,0250,020 to 0,0401,00 to 1,300,25
12CrMo40,10 to 0,150,300,60 to 0,900,0250,0250,90 to 1,200,15 to 0,250,25
18CrMo40,15 to 0,210,300,60 to 0,900,0250,0250,90 to 1,200,15 to 0,250,25
18CrMoS40,15 to 0,210,300,60 to 0,900,0250,020 to 0,0400,90 to 1,200,15 to 0,250,25
20MoCr40,17 to 0,230,300,70 to 1,000,0250,0250,30 to 0,60 0,40 to 0,50 0,25
20MoCrS40,17 to 0,230,300,70 to 1,000,0250,020 to 0,0400,30 to 0,600,40 to 0,500,25
Elements not quoted in this table should not be intentionally added to the steel without the agreement of the purchaser,except those intended for finishing the heat.All reasonable precautions shall be taken in order to prevent the addition of such elements from scrap or other materials used in the production process,which can affect the hardenability, mechanical properties and applicability To improve the performance of cold heading,it is possible to add Al:0,020 %to 0,050 % a Maximum values unless otherwise indicated. b In the case of steels with hardenability requirements (see Tables B.6 and B.Z),minor deviations from the specified limits are permitted (with the exception of sulfur and phosphorus),provided that they do not exceed 0,01 %for carbon and the values indicated in Table 2 for the other elements. c A lower silicon content or a specific silicon range may be agreed at the time of ordering

3. mechanical properties

Table B.4 -Mechanical properties of nitrogen-containing alloy steel grades

    Steel nameDiameterDelivery condition
  +AR          +AC or +AC+PE    +AR+C    +AR+C+AC    +AR+C+AC+LC    +AC+C  
above mmup to mmRm max. MPaZa min %Rm max. MPaZ min. %Rm max. MPaZ min %Rm max. MPaZ min. %Rm max. MPaZ min. %Rm max. MPaZ min. %
  18MnB425    5006454062  
510580555006468053480645206260059
1040580555006467053480645206259059
  22MnB425    5206456062 
510600555206272053500645406263059
1040600555206271053500645406262059
a The values are given only for information.

4. Hardening requirements

Table B.6-Hardness limits for steel grades with standard hardenability (+H grade)

  Steel nameSymbolAustenitizing temperature ℃±5℃Limits of rangeHardness HRC at a distance from quenched end of test piece(in mm)of
1,535791113152025303540
18MnB4+H890max.464544413935322821   
min.4038373021     
22MnB4+H880max.49484745423935322420  
min.4341403223    
17Cr3+H880max47444033292725242321 
17CrS3min.39352520   
20Cr4+H900max.49484642383634322927262423
20CrS4min.413831262321-
16MnCr5+H870max.47464441393735333130292827
16MnCrS5min.393631282421    
16MnCrB5+H870max.47464441393735333130292827
min.393631282421     
20MnCrS5+H870max.49494846434241393735343332
min.41393633302826252321 
12CrMo4+H870max.44434138343028272321 
min.3634302622  
18CrMo4+H880max.47464542393735343129282726
18CrMoS4min.3937343027242221     
20MoCr4+H910max.49474441383533312826252424
20MoCrS4min.413731272422     
10NiCr5+H880max.413937343230  
min32272422   
12NiCr3-2+H870max.4340352621  
min.373225    
17CrNi6-6+H870max.47474645434241393735343433
min.39383635323028262422212020
20NiCrMo2-2+H880max.49484542363331302725242423
20NiCrMoS2-2min.413731252220       
线材捆扎示例
Example of wire bundling
成品标签示例
Example of finished product label
卷材的卷绕方式
Coil winding method

Example of outer packaging

端面木板包装
End board packaging
缠绕包装
winding packaging
PP布袋套袋包装
PP bag packaging
线架包装
Wire rack packaging
栈板包装
Pallet packaging

Group technical resources

fastener-wire.com ↗