diameter: 0.40-46mm
tensile strength: refer to technical information

Shanghai Chuang Group is a benchmark company in China focusing on cold-rolled high-quality steel wire. The entire management team has 20 years of industry experience. We have established good relationships with many first-level suppliers in the automotive industry, and all steel wires come from brand steel mills. All orders are 100% traceable.

img1 img1 img1

Specification

+AC or +AC+PE

+AC+C+AC

+AC+C+AC+LC

img1 img1 img1

Specification

-:continuous and smooth

-:No seams, overlaps, pits, scratches and drawing scars

-:free from rust

img1 img1 img1
img1 img1 img1

Specification

-:automobile industry

-:construction industry

-:machinery industry

-:other industries

img1 img1 img1
Case Study

Products & Service

Related Products

46Cr2 CHQ steel wire

Prepainted Aluminium Coil

46Cr2 CHQ steel wire

Prepainted Aluminium Coil

46Cr2 CHQ steel wire

Prepainted Aluminium Coil

1. Delivery terms combination

Table C.1 -Combination of heat treatment conditions, product form and applicable requirements at the time of delivery

Heat-treatment condition at deliverySymboProducts form aApplicable requirements in cases where the steel concerned has been ordered with reference to the steel names indicated in
Wire rodBarWireTables C.2,C.3,C.4, C.5 or C.6Tables C.2,C.3,C.4,C.5,C,6,C.Z C.8 or C.9Tables C.2,C.3,C.4,C.5,C.6 or C.10Optional
As hot-rolled or peeled+AR or +PEXXXChemical compo- sition as speci- fied in Tables C.2 and C.3Me- chanical properties as spec- ified in Tables C.4. C.5 and C.6Chemical compo- sition as speci- fied in Tables C.2 and C.3Me- chanical properties as spec- ified in Tables C.4, C.5 and C.6Values for harden- ability according to Tables C.Z C.8 and C.9Chemical compo- sition as speci- fied in Tables C.2 and C.3Me- chanical properties as spec- ified in Tables C.4. C.5 and C.6Mini- mum core hardness and max- imum diameter accord- ing to TableC.10Supplementa- ry or special requirements as specified in Annex Eb
Cold drawn+AR +CXX
Cold drawn + spheroidized+AR+C+ ACXX
Cold drawn + spheroidized + skin passed+AR+C  +AC +LCXX
Spheroidized or spheroidized +  peeled+AC or +AC+PEXXX
Spheroidized + cold drawn+AC+CXX
Spheroidized+ cold drawn +spheroidized+AC+C+ ACXX
Spheroidized + cold drawn +sphe- roidized +skin passed+AC+C+ AC+LCXX
OthersOther delivery conditions may be agreed at the time of ordering
a    X=applicable,—=not applicable b If agreed at the time of the enquiry and order.

2. chemical composition

Table C.3-Chemical composition of nitrogen-containing alloy steel grades for quenching and tempering (suitable for casting analysis)

Steel name b% mass fraction
CSi cMnPSCr dMoBCu
17B20,15 to 0,200,300,60 to 0,900,0250,0250,30 0,0008 to 0,0050,25
23B20,20 to 0,250,300,60 to 0,900,0250,0250,30 0,0008 to 0,0050,25
28B20,25 to 0,300,300,60 to 0,900,0250,0250,30——0,0008 to 0,0050,25
33B20,30 to 0,350,300,60 to 0,900,0250,0250,300,0008 to 0,0050,25
38B20,35 to 0,400,300,60 to 0,900,0250,0250,300,0008 to 0,0050,25
23MnB30,21 to 0,250,150,80 to 1,000,0150,0150,25 to 0,350,0008 to 0,0050,25
17MnB40,15 to 0,200,300,90 to 1,200,0250,0250,300,0008 to 0,0050,25
20MnB40,18 to 0,230,300,90 to 1,200,0250,0250,30 0,0008 to 0,0050,25
23MnB40,20 to 0,250,300,90 to 1,200.0250,0250,300,0008 to 0,0050,25
27MnB40,25 to 0,300,300,90 to 1,200,0250,0250,300,0008 to 0,0050,25
30MnB40,27 to 0,320,300,80 to 1,100,0250,0250,300,0008 to 0,0050,25
36MnB40,33 to 0,380,300,80 to 1,100,0250,0250,300,0008 to 0,0050,25
20MnB50,17 to 0,230,301,10 to 1,400,0250,0250,300,0008 to 0,0050,25
23MnB50,20 to 0,260,301,10 to 1,400,0250,0250,300,0008 to 0,0050,25
26MnB50,23 to 0,290,301,20 to 1,500,0250,0250,300,0008 to 0,0050,25
34MnB50,31 to 0,370,301,20 to 1,500,0250,0250,300,0008 to 0,0050,25
37MnB50,35 to 0,400,301,15 to 1,450,0250,0250,300,0008 to 0,0050,25
30MoB10,28 to 0,320,300,80 to 1,000,0250,0250,30e0,08 to 0,120,0008 to 0,0050,25
provided that they do not exceed 0,01 %for carbon and the values indicated in Table 2 for the other elements.
 
Elements not quoted in this table should not be intentionally added to the steel without the agreement of the purchaser,except those intended for finishing the heat.All reasonable precautions shall be taken in order to prevent the addition of such elements from scrap or other materials used in the production process,which can affect the hardenability, mechanical properties and applicability To improve the performance of cold heading,it is possible to add Al:0,020 %to 0,050 %.
a b
 
Maximum values unless otherwise indicated. In the case of steels with hardenability requirements (see Table C.8),minor deviations from the specified limits are permitted (with the exception of sulfur and phosphorus)   c   Lower silicon contents may be agreed at the time of ordering,in which case due consideration should be given to the effects that could result for what concerns the specified properties such as,for example,hardenability. d Where a maximum chromium content of 0,30 %is specified,a minimum level may also be agreed at the time of enquiry and order e  In order to obtain a core hardening for the steel grade 30MoB1,the lower limit of Cr shall be 0,15 %and may be agreed at the time of enquiry and order.For certain applications, the higher limit for Cr may also be lowered by agreement at time of enquiry and order.

3. mechanical properties

Table C.5 -Mechanical properties of steel grades without B alloy

    Steel nameDiameterDelivery condition
+AC or +AC+PE+AC+C+AC+AC+C+AC+LC
above mmup to mmRm max. MPaZ min %Rm max. MPaZ min. %Rm max. MPaZ min. %
37Mo225  5606160059
540570595506159059
38Cr225  5906263060
540600605806262060
46Cr225  6106065058
540620586006064058
34Cr4255706461062
540580625606460062
37Cr425  5806262060
540590605706261060
41Cr4 41CrS4256106065058
540620586006064058
25CrMo4 25CrMoS425  5706261060
540580605606260060
34CrMo4255906263060
540600605806262060
37CrMo425  6106265060
540620606006264060
42CrMo4 42CrMoS425  6206066058
540630586106065058
41CrNiMo2 41CrNiMoS2256406068055
540————6406068055
34CrNiMo625————7106075058
540720587006074058
41NiCrMo7-3-2257106075058
540720587006074058

4. Hardening requirements

Table C.7-Hardness limits for non-B steel grades with specified (normal) hardenability (+H grade)

  Steel name  Sym- bolAustenitizing temperature °℃±5℃  Limits  of range                                                 Hardness HRC        at a distance from quenched end of test piece(in mm) of
12345678910111315202530
C35EC+H870max.585755534941343128272625242320
C35RC+Hmin.484033242220       
C45EC+H850max.61605957534739343130292827262524
C45RC+Hmin51463527252423222120 
 at a distance from quenched end of test piece(in mm) of
1,5357911131520253035404550 
37Mo2+H850max.59575347413632292725  
min.5148413327262220       
38Cr2+H850max.595754494339373532302725242322
min.51463729252220        
46Cr2+H850max.636157524642403835333129282726 
min544940322825232220      
34Cr4+H850max.575756545249464439373534333231 
min.4948454135322927232120   
37Cr4+H850max.595958575552504842393736353433
min.515048443936333126242220    
41Cr4+H850max.616160595856545246424038373635 
41CrS4min,535250474137343229262321  
25CrMo4+H850max.525251504846434137353332313131 
25CrMoS4min.4443403734322927232120 
34CrMo4+H850max.575757565554535248454341404039 
min.494948454239363430282726252424
37CrMo4+H850max606060595856555451484645   ——
min.525049474543403734323130    
42CrMo4+H850max.616161606059595856535148474645 
42CrMoS4min535352514943403734323130302929 
线材捆扎示例
Example of wire bundling
成品标签示例
Example of finished product label
卷材的卷绕方式
Coil winding method

Example of outer packaging

端面木板包装
End board packaging
缠绕包装
winding packaging
PP布袋套袋包装
PP bag packaging
线架包装
Wire rack packaging
栈板包装
Pallet packaging

Group technical resources

fastener-wire.com ↗